  • Item:Printing Binder EM-800

    ◎Technical Index
    Appearance: Translucent liquid.                    Composition: self-cross linking acrylate polymer
    Ionic Property: Anionic                            PH Value: 6~7
     
    ◎Properties and characteristics
    Strong fixation ability & good fastness.
    Rich color value and vivid luster, sharp outline.
    Fine filteration, screen choking free property, non-stick to blades.
    High quantity & reasonable price.
    Printed fabric achieves environmental protection requirement.
     
    ◎Application
    1. Extremely applicable for plush, blanket, carpet etc. Printing result of hand feeling and effect are very close to as received in reactive dyes printing.
    2. Applicable for printing on towel, bath towel, woolen sweater and other kind of terry fabrics and synthetic fiber and other blended fabrics。
    3. Suitable for printing process with roller, rotary screen, flat screen, handy screen or praying printing.
    Printing paste formula

    printing thickener EM-PTE

    printing binder

    pigment paste

    water

    TOTAL

    1.5%-2%

    10%-20% (depends to actual situation)

    X%

    Y%

    100%

    (If the printing paste not thick enough, add some thickener, stir good enough is ok)
     
    ◎Operation process
    1. Prepare printing paste with above-described stock paste mixed with pigment paste and color fixing agent.
    2. Use appropriate printing mesh (80-120 mesh) to printing and then dry afterwards
    3. It will give better result after baking fixation for 3-5 minutes under 130-150°C
     
    ◎Package
    60kg or 125kg net in plastic drum.
     
    ◎Storage
    It can keep for one year under 5-35°C. Avoid exposure or frozen. It can be stored one year. 
     
    ◎Notes
    1. Do needful testing and identify printing result required every time before use.
    2. A suitable color fixing agent may do good to color fastness and rubbing fastness. Don’t mix the product with cationic printing paste or auxiliaries.
    3. Baking fixation should be done only when printed cloth is dry entirely, which will enhance result of color fastness and rubbing fastness as well.
    4. For fastness testing, it can be done after 24-48 hours.
    5.The newly dried printing surface after baking fixation feels a little hard, but will start getting soft after some time (on the second day).